A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Resist Coating Large Scale Conformal/Ogave surfaces
Resist Coating Large Scale Conformal/Ogave surfaces
2007-02-20
David Casale
2007-02-20
Bill Moffat
2007-02-20
Cain, Mike
2007-02-20
Rick Williston
2007-02-21
David Casale
Resist Coating Large Scale Conformal/Ogave surfaces
Bill Moffat
2007-02-20
David,
      I think we have talked about a different problem.  The goobers are
a function of your coater and how you operate it.  If you are using wet
HMDS sprayed on before resist coating the most common problem is a drip
from the HMDS nozzle at the wrong time.  If this is the problem the
boogers are radial with a nearly round head say 10 microns in diameter
and a comet tail out to the edge of the wafer.  They can also be a
function of your coater exhaust.  If you ramp up fast and use a high
speed camera you will see a mist of resist over the wafer as you ramp
up.  If your exhaust is poor some of these resist balls will settle back
on the wafer. I did an interesting experiment with an old 4 track system
plotting round defects.  With the exhaust at the back, the back track
had no defects.  The next to the back had say dozens, the next track had
hundreds and the front track the farthest from the exhaust had
thousands.  Give me a call if you can and we can talk resist track
problems.
Bill Moffat, CEO
Yield Engineering Systems, Inc.
2185 Oakland Rd., San Jose, CA  95131
(408) 954-8353
cell 408 590 4577
[email protected]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation
Addison Engineering