MEMSnet Home: MEMS-Talk: Resist Coating Large Scale Conformal/Ogave surfaces
Resist Coating Large Scale Conformal/Ogave surfaces
2007-02-20
David Casale
2007-02-20
Bill Moffat
2007-02-20
Cain, Mike
2007-02-20
Rick Williston
2007-02-21
David Casale
Resist Coating Large Scale Conformal/Ogave surfaces
Cain, Mike
2007-02-20
Hello David,

Some ideas on where to look......  Is the resist automatically dispensed
or "hand poured (or pipette)?"  Are the defects visible after coat but
before the softbake?  Did the process ever work?

Some of the problems I have encountered:

Dirty coat bowl stirring up dried resist particles.
Poor exhaust - again causing dried resist particles to fly around in the
bowl.
Poor resist dispense - dried resist on the dispense nozzle (or filter or
pump or whatever method used to dispense the chemical). Acetone
splashback caused by edge bead removal or similar.

Feel free to contact me directly; [email protected] for other
suggestions.

Cheers,

Mike
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
Harrick Plasma, Inc.
MEMS Technology Review