MEMSnet Home: MEMS-Talk: pmma lithography
pmma lithography
2007-02-25
Chen Han Lee
2007-02-25
[email protected]
2007-02-26
Jim Beall
2007-02-26
Chris Park
pmma lithography
[email protected]
2007-02-25
PMMA is used mostly for electron beam lithography (EBL).  I don't think it
responds to UV light; although, I've never exposed PMMA.

David Fozdar

University of Texas at Austin
Deparment of Mechanical Engineering - Thermal/Fluids Systems
Center for Nano Molecular Science and Technology (CNM)

Quoting Chen Han Lee :

> hi all,
>
> i am wondering if pmma can be patterned by UV radiation?
> I know that the most common exposure source is X-ray, but is there others?
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
MEMS Technology Review
University Wafer