MEMSnet Home: MEMS-Talk: lihography problem
lihography problem
2007-02-26
abhaya joshi
2007-02-27
P.E.M. Kuijpers
lihography problem
P.E.M. Kuijpers
2007-02-27
Hello,

Spraycoating would solve this problem or when you have a conductive layer
an Electro Disposable resist (Eagle) is also an option.


Peter Kuijpers
MiPlaza
DTS/TFF
High Tech Campus 04
Room: WAGp5-11
5656 AE Eindhoven
The Netherlands

Phone.:  (+31 40 27) 98904 (mobex)
mobile:(+31) 06-12507027
fax.:     [+31 40 27) 44769
mailto:[email protected]


"abhaya joshi" 
Sent by:
[email protected]
26-02-2007 05:49
Please respond to
General MEMS discussion 

To
[email protected]
cc

Subject
[mems-talk] lihography problem
Classification

hi friends
i have etched si wafer for 30 um using KOH. the cavities are of size 1000
X
2000 um.
but when i am doing lithography on this surface, the photoresist is not
covering all the  area, specially from top side of top surface.
i have tried with thicker photoresist (at 2000 RPM), but it is not
working.
i am using HNR120 (-ve PR) and S1813 (+ve PR)
please suggest me to solve this problem.
-abhay joshi
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Nano-Master, Inc.
MEMStaff Inc.