MEMSnet Home: MEMS-Talk: Wet etching Gold
Gold on SU-8
2007-02-26
Yue Mun Pun, Jeffrey
2007-02-26
Kevin Paul Nichols
2007-03-05
Yue Mun Pun, Jeffrey
Wet etch chemistry for evaporated titanium
2007-02-27
Yue Mun Pun, Jeffrey
2007-02-27
Brent Garber
Wet etching Gold
2007-03-01
Yue Mun Pun, Jeffrey
Wet etching Gold
Yue Mun Pun, Jeffrey
2007-03-01
Hi,
I am trying wet etch gold film from 60nm down to 30nm.  My lab has 2 available
chemistries, KCN and KI:I2 chemistries.  Due to the potential toxicity of KCN, I
have chosen to use the KI/I2 chemistry in the proportion KI:I2:H2O = 4:1:40ml.
I have tested this chemistry on 80nm of gold evaporated on PDMS.  In the
literature it was reported that KI/I2 chemistry in the proportion I used can
etch gold at a rate of 1 micron per min, but in my trial, I have discovered that
the 80nm gold film takes 6 times longer to remove.  The removal of the gold is
not complete as there is still a thin layer of gold film left behind.
Can anyone suggest a more effective and controllable way to wet etch gold?

Mr. Jeffrey Mun Pun YUE
???
Division of Bioengineering
Block E3, #05-18, Nanobioanalytics Lab
9 Engineering Drive 1
National University of Singapore
Singapore 117576
Tel: (65) 65165985, Fax: (65) 68723069
E-mail:  [email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
University Wafer
Tanner EDA by Mentor Graphics