MEMSnet Home: MEMS-Talk: Depositing metals onto plastics and SU-8
Depositing metals onto plastics and SU-8
2007-03-01
Jon Fox
2007-03-01
Brent Garber
2007-03-03
Roger Shile
2007-03-03
Mantavya Sinha
2007-03-03
Kirt Williams
2007-03-01
Mohamad Hajj Hassan
2007-03-02
Samadhan Bhaulal Patil
2007-03-03
[email protected]
2007-03-04
[email protected]
2007-03-05
Jesse D Fowler
2007-03-06
Yue Mun Pun, Jeffrey
Depositing metals onto plastics and SU-8
Jon Fox
2007-03-01
I'm using resistive evaporation to put down various metals onto SU-8 and
onto plastic substrates and am seeing significant sample heating which
seems to be causing as little as some reflow or as much as unidentified
hazy thin films around the sample.

I will be trying to move my metal source (resistive canoe) away from the
sample to alleviate this, but I was wondering what the preferred method
of depositing metals onto polymers was: resistive, e-beam bombard, or
sputtering?

Thanks,
-Jon Fox

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Addison Engineering
Process Variations in Microsystems Manufacturing