A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Depositing metals onto plastics and SU-8
Depositing metals onto plastics and SU-8
2007-03-01
Jon Fox
2007-03-01
Brent Garber
2007-03-03
Roger Shile
2007-03-03
Mantavya Sinha
2007-03-03
Kirt Williams
2007-03-01
Mohamad Hajj Hassan
2007-03-02
Samadhan Bhaulal Patil
2007-03-03
[email protected]
2007-03-04
[email protected]
2007-03-05
Jesse D Fowler
2007-03-06
Yue Mun Pun, Jeffrey
Depositing metals onto plastics and SU-8
[email protected]
2007-03-04
Mantavya,

Go to the back of the classroom with Roger.  You can cool a substrate in an
e-gun evaporation if you want.  Sputtering always produces heat to the
substrate.  Roger brought up the charge (source) heat, who cares?
Substrate heat was the issue.

Brent


You are right Roger. E-Beam is not going to be a cool process. In my
experience Sputtering should give you near room temperature (RT +
10'C-15'C) deposition.

Cheers

Mantavya Sinha
PhD Student
Dept of ECE
NUS


Contrary to many postings here, E-beam evaporation is thermal
evaporation; the charge is not cool by any means.

Roger Shile
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
University Wafer
MEMS Technology Review