Try a metal that forms a native oxide, e.g. chrome or titanium.

-Mike Martin

>>> "Leyla Soleymani"  3/5/2007 1:28 PM >>>
Hi,

I would like to use  electron beam evaporation in order to evaporate silica
on a gold substrate for isolation purposes. I have tried this but I did not
get adhesion between SiO2 and gold. Does anyone have any suggestions to what
adhesion layer and how much of it I should use in order to acheive an SiO2
layer of 100 nm on sputtered gold. I do not have a CVD system so i need to
use thermal evaporation.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Addison Engineering
Process Variations in Microsystems Manufacturing