Leyla Soleymani
2007-03-06
l ll
Wet Etching SiO2 using PMMA
l ll
2007-03-06
Hi

  I dont think PMMA can resist HF or BOE. It certainly doesnt have resistance to
flourine plasma in the RIE.

  Sharukh

Leyla Soleymani  wrote:
  Hi,
Does anyone know if PMMA can be served as a wet etch mask for BOE of
SiO2. I have 520nm of SiO2 on Glass/Ti/Gold and I have access to
Microchem PMMA 950,000 A2. Is it possible to use the PMMA as a mask to
etch the oxide using HF. If so, does anyone know a sample procedure.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Harrick Plasma, Inc.