A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Methods to make thick resist layer
Methods to make thick resist layer
2007-03-06
[email protected]
2007-03-07
P.E.M. Kuijpers
2007-03-08
[email protected]
2007-03-08
Yue Mun Pun, Jeffrey
2007-03-08
Hongzhi CHEN
Methods to make thick resist layer
P.E.M. Kuijpers
2007-03-07
Hi all,

Try a double spincoat process with AZ4562 or AZ9260.
Resist layers up to 70µm were achieved.

Regards,
Peter Kuijpers
MiPlaza
DTS/TFF
High Tech Campus 04
Room: WAGp5-11
5656 AE Eindhoven
The Netherlands

Phone.:  (+31 40 27) 98904 (mobex)
mobile:(+31) 06-12507027
fax.:     [+31 40 27) 44769
mailto:[email protected]

--------------------------------------
[email protected]
Sent by:
[email protected]
06-03-2007 20:37

Subject
[mems-talk] Methods to make thick resist layer
Classification

Hi all,
   I am wondering if there is an easy way to make features higher than
50 um with a 10 um gap. I've tried su8 which can give thick resist in
one spin, but the gap didn't come out (using transparency mask). With
SPR or AZ resist, the gap can be made successfully, but it seems hard
to go higher than 50 um. I am wondering if anyone had similar
experience and any suggestion is gratefully acknoledged.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review
Mentor Graphics Corporation