Hi all,

I want to electroplate a 3µm thick Au layer onto a 10µm thick Ni
layer.
This Ni layer was also electroplated.
What kind of pre-treatment should I use, to obtain a good adhesion between
the Au and Ni layer??

Thanks in advance.


Peter Kuijpers
MiPlaza
DTS/TFF
mailto:[email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
MEMStaff Inc.