A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: hi for help about the develop
hi for help about the develop
2007-03-13
[email protected]
2007-03-13
Shay Kaplan
2007-03-14
[email protected]
2007-03-14
Shay Kaplan
2007-03-14
Robert Black
2007-03-15
Joseph Grogan
2007-03-13
Joseph Grogan
2007-03-14
Avi Laker
hi for help about the develop
Shay Kaplan
2007-03-13
Don't bake over 100 deg before exposure - 95 deg is better
Shay

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of [email protected]
Sent: Tuesday, March 13, 2007 6:12 AM
To: [email protected]
Subject: [mems-talk] hi for help about the develop

 I spin S1813 at 4000rpm 45s.
Then hot bake 120Degree 10min
Exposure 10s, then develop 30s.After 30s, I can't see anything.
Why???
All paper recommend the develop time 30s.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
The Branford Group
University Wafer