Sorry, I didn't see the message until just now. I was trying to get as
high as possible, so su8 2025 was spun at 1000 rpm. The sample was
settled for 5 min and heated on hotplate with temperature ramping up
from room temperature to 95 degree. After 10 min at 95 degree,
temperature is ramped down before 5 min exposure at 4.5 mW/cm^2. The
post exposure baking is the same as pre-bake. Basically, the 10 um gap
is still filled by su8 after development.
Thanks in advance for your suggestion.

On 3/7/07, Sebastien Jiguet  wrote:
>
>  Dear Liu Yu,
>
>  What was your SU-8 process to pattern 50 µm thick film?
>  Normally it should be possible to obtain 10 µm gap depending on the
> interface nature.
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
The Branford Group
Process Variations in Microsystems Manufacturing