Hello,
Abbe refractometers are common instruments used to measure the refractive
index of liquids. A web search will provide a list of vendors.
Cheers!
Chris Bliss

-----Original Message-----
From: Peng Li (Paul) [mailto:[email protected]]
Sent: March 19, 2007 11:55 AM
To: [email protected]
Subject: [mems-talk] measure refractive index

Hey all,

Does anybody know what kind of instrument can be used to measure the
refractive index of liquid? Which vendor and what products do you recommend
for use?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
Mentor Graphics Corporation
MEMStaff Inc.