A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Au plating on Ni layer
Au plating on Ni layer
2007-03-28
P.E.M. Kuijpers
2007-03-28
David Nemeth
2007-03-28
Bob Forman
Au plating on Ni layer
Bob Forman
2007-03-28
Go directly from the Ni plating to Di rinse to Gold plating with no dwell
in air in between (keep the wafer wet all the time).. this sill prevent Ni
oxides from forming.  Also Au will immerse onto Ni, so make sure the
plating power is applied immediately when immersed in the gold bath...
good luck..

Bob Forman | Business Manager, Advanced Packaging
Rohm and Haas Electronic Materials | Packaging and Finishing Technologies
10414 78th ave NW | Gig Harbor, WA 98332| Phone: 425-785-9817 |
http://electronicmaterials.rohmhaas.com


"P.E.M. Kuijpers" 

Subject [mems-talk] Au plating on Ni layer

Dear all,

What kind of pre treatment of the Ni layer must I use to obtain a good
adhesion of the plated Au layer??
Ni was plated using a NiCl solution, Au was plated using Aurofab BP, but
adhesion was very bad.
Thanks,

Peter Kuijpers
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Addison Engineering
Process Variations in Microsystems Manufacturing