MEMSnet Home: MEMS-Talk: SU-8 adhesion on NOA61
SU-8 adhesion on NOA61
2007-04-05
[email protected]
KOH etch
2007-04-07
Andrea Mazzolari
SU-8 adhesion on NOA61
[email protected]
2007-04-05
Hi,

We have been struggling with the adhesion of SU-8 on NOA61 (Norland Optical
Adhesive a UV curable epoxy). We are trying to make optical waveguide in
SU-8 with NOA61 as the cladding layer. We tried using HMDS to promote
adhesion between the two polymers but so far unsuccessful.

In a typical experiment, we spin NOA61 on clean Si wafer, and UV expose it
to harden the epoxy. We then spin SU-8 on this. Without adhesion promoter,
SU-8 simply flies off. With HMDS, some SU-8 sticks, though the thickness is
far less than what we should get at that spin speed.

Any help in this regard will be greatly appreciated. Thanks in advance.

Satyanarayan

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
Nano-Master, Inc.
Harrick Plasma, Inc.