MEMSnet Home: MEMS-Talk: silicon rich nitride wet etch
silicon rich nitride wet etch
2007-04-12
Ciro Chiappini
2007-04-12
Andrea Mazzolari
Re: silicon rich nitride wet etch
2007-04-12
Ciro Chiappini
2007-04-13
PRAMOD GUPTA
2007-04-13
[email protected]
2007-04-15
Kirt Williams
silicon rich nitride wet etch
Andrea Mazzolari
2007-04-12
Hello Ciro,
i never worked with your resist, i usually use Shipley S1813 and BHF wet
etch solution (HF:NH4F, 1:7). S1823 peel off after different hours.
Let me know if you need details on how to process S1813.

Best regards,
Andrea



> Hi
>
> I have to etch a 2000Ã… thick silicon rich nitride film under a
> photoresist
> (AZ5209) mask. I need to get a nitride mask since the next step is
> electrochemical etching in EToH:HF 3:7. I am currently RIE etching it, but
> the process is very time consuming.
>
> I tried wet etch both HF:H2O 1:10 AND HF:HCL 1:1 but the resist gets
> peeled
> off in few minutes.
>
> Do you have any alternative recipe to suggest?
>
> Thanks
>
> Ciro Chiappini
> UT-Austin/UT-Health Science Center Houston
> Biomedical Engineering Department
> Dr. Mauro Ferrari Nanomedicine Lab
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
University Wafer
MEMS Technology Review