Etching of intermetallic CuAu
2007-04-17
P.E.M. Kuijpers
Al oxide
2007-04-18
Hongzhi CHEN
Etching of intermetallic CuAu
P.E.M. Kuijpers
2007-04-17
Hi all,

After Cu plating on a TiAu seedlayer I etched the seedlayer in a KI/I2
solution, but a lot of residues remained, maybe as a result of formed CuAu
intermetallic(?)
Analyses showed a large Cu contant of these residues. Wet etching in Cu
etch  and afterwards  Ion Beam Etching, didn't solve this problem yet.
Do you have any suggestion for this?

Thanks,
Peter Kuijpers
MiPlaza
DTS/TFF

mailto:[email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group
Tanner EDA by Mentor Graphics