A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: will the SOI fabrication process affect the anodicbonding
will the SOI fabrication process affect the anodicbonding
2007-04-21
Brubaker Chad
RE: RE: [mems-talk] will the SOI fabrication process affect the anodic bonding
2007-04-26
matthew king
will the SOI fabrication process affect the anodicbonding
Brubaker Chad
2007-04-21
SOI wafers can still anodically bond, although it is somewhat more difficult,
depending on oxide thickness. If the oxide is thin you may be able to get away
with simply increasing the voltage used.

If the oxide is too thick, you'll probably need to make a grounding contact
directly to the SOI surface - this is most easily accomplished by rotating a
flat marked glass 90º away from  the flat of the SOI, and making a grounding
contact directly to the edge exposed at the flat of the glass.

Best Regards,
Chad Brubaker

EV Group       invent * innovate * implement
Senior Process Engineer - Technology - Tel:  480.727.9635, Fax:  480.727.9700
e-mail: [email protected], www.EVGroup.com

-----Original Message-----
From: [email protected] [mailto:[email protected]] On
Behalf Of matthew king
Sent: Thursday, April 19, 2007 6:49 AM
To: [email protected]
Subject: [mems-talk] will the SOI fabrication process affect the anodicbonding

Hi all,

The wafer supplier offer SOI wafers fabricated in several ways, including SIMOX
and bonding. As I need to anodically bond the SOI to glass, I wonder if the
intermediate SiO2 would make the bonding impossible.So my first question is:If
the choice of SOI fabrication process would affect the bonding process,or I just
need to pay attention to specifications like resistivity and SiO2
thickness(<100n?)?

  Both silicon layers of SOI is needed. They both have low resistivity but the
top silicon is much thicker than the hander layer.My second question is: Can I
just buy a double side polished SOI wafer and use the handle layer as the device
layer?Will this bring trouble to processes?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
University Wafer
Mentor Graphics Corporation