MEMSnet Home: MEMS-Talk: silicon nitride on germanium
Etching SiO2
2007-04-20
Huy
silicon nitride on germanium
2007-04-21
Andrea Mazzolari
silicon nitride on germanium
Andrea Mazzolari
2007-04-21
Hi all,
i deposited LPCVD silicon nitride on 4'' germanium wafers. I obtained a
very very bad uniformity of silicon nitride film.
Here are the process conditions:
DCS flow rate: 30sccm
NH3 flow rate: 150sccm
pressure: 200mtor
temperature: 750 °C
When depositing on silicon wafers using the same parameters i obtain a
good uniformity. Is there a way to obtain good uniform also on germanium
wafers ?

Best regards,
Andrea
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
University Wafer
The Branford Group
Addison Engineering