Indusekhar,

Thank you for your answer! I have SOG on a Al2O3
coated structure. After the process that requires
baking
of SOG, I want to reveal the Al2O3 surface.
Unfortunately, HF removed both layers. Maybe I need to
try lower concentration. Are there any other recipes
having better etching result on this combination?

Dong


From: "Indusekhar" 
To: [email protected]
Date: Wed, 25 Apr 2007 09:46:00 +0530
Subject: [mems-talk] SOG removal

SOG removal:
If you have not baked , it can be removed with IPA.
IF SOG is baked after coating, you can etch with
buffered HF solution.

Indusekhar

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.