A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Au electroplating
Au electroplating
2007-05-09
kris
2007-05-09
David Nemeth
2007-05-10
Shay Kaplan
2007-05-10
P.E.M. Kuijpers
2007-05-10
David Nemeth
2007-05-10
David Roberts
2007-05-11
P.E.M. Kuijpers
2007-05-11
David Roberts
2007-05-14
P.E.M. Kuijpers
Miniature Hot Press for Plastic Microdevice bonding
2007-05-14
Heiko van der Linden
2007-05-14
David Roberts
2007-05-14
Mo Kebaili
Au electroplating
David Roberts
2007-05-10
Hi Peter,
Cathodic activation at 20mA/cm2 in 10%sulfuric. Keep wet. Plate gold.
Regards,
David Roberts (Wafer Plating Specialist)
Prodigy Surface Tech
Santa Clara, CA

-----Original Message-----
From: P.E.M. Kuijpers [mailto:[email protected]]
Sent: Wednesday, May 09, 2007 10:50 PM
To: General MEMS discussion
Subject: Re: [mems-talk] Au electroplating

Hello Kris,

We did  also electroplating of Au (sulphite based)on Ni, but we observed a
very bad adhesion of Au onto the Ni seedlayer.
Did you observed this also or do you have a special pre-treatment to
overcome this?



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
University Wafer
Addison Engineering