A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: XeF2 Etching Silicon
Quartz Etching
2007-05-17
Sreemanth M Uppuluri
2007-05-17
Gareth Jenkins
2007-05-17
Bill Moffat
2007-05-18
Andrea Mazzolari
2007-05-18
Kirt Williams
XeF2 Etching Silicon
2007-05-18
Bin Liu
2007-05-18
ChungHao Chen (Joseph)
2007-05-18
P.D. Floyd
2007-05-18
Kirt Williams
Fused Quartz Cleaning
2007-05-30
Sreemanth M Uppuluri
2007-05-30
Julie Houser
2007-05-31
shay kaplan
2007-05-21
Nodes Norbert
XeF2 Etching Silicon
ChungHao Chen (Joseph)
2007-05-18
Hi Bin,

You might not have enough of XeF2 gas to react with Si. Try to reduce the cycle
time such as 1 min and run the etching for many cycles. On the other hand, The
total area needed to be etched may be large which causes the slow etch rate as
well.

Best,

Joseph

--
ChungHao Chen (Joseph)
Research Assistant
Purdue University
School of Electrical and Computer Engineering
EE Building Box 114
465 Northwestern Avenue
West Lafayette, IN 47907-2035
email: [email protected]



Quoting Bin Liu :

> Dear All,
>
> I plan use XeF2 etch silicon. The XeF2 is designed to go through several
> 3*5um holes of photoresist and then etch away the silicon underneath. I
> want the etched area to be 20um in radius. I heated up the XeF2 to
> 75C-95C during the etching process, the pressure during etching is
> around 4 torr, I flush the XeF2 every 10 min, and got the sample sitting
> in the gas for 40 min, but I still get very limited etching area through
> the holes. I wonder if anyone have experience on XeF2 etching silicon,
> can you give me some suggestion? the temperature? the pressure? or is it
> because the holes are so small that limit the etching area?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.