MEMSnet Home: MEMS-Talk: How to etch SU8 from Nickel structure?
How to etch SU8 from Nickel structure?
2007-05-14
Simon Zhang/gcemarket
2007-05-14
Dubnisheva, Anna
2007-05-19
Shigetomo SHIKI
How to etch SU8 from Nickel structure?
Shigetomo SHIKI
2007-05-19
> Anyone knows good wet or dry etching method for etching SU8 from Nickel
> structure ?

I have some experience of SU8 dry etching of 5um depth and 2um size with
thin (<1um) metal mask.  I hope my recipe help you.

You can remove SU8 with O2 RIE.  Pure O2 etching is anisotoropic.  The
rate was moderate(200nm/min, 30Pa O2, 200W RF) in my chamber.  You may
found some residual filaments of sub-um diam, um length after RIE
process (the filaments may not be seen with optical microscope).  Side
wall is not smooth in the scale of sub-micrometer.

When 5-10% SF6 is added, etching rate is higher than the rate of pure O2
etching.  Etching profile is isotoropic, side wall is smooth, and the
amount of residual is small.

Best regards,

Shigetomo Shiki

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
Nano-Master, Inc.
MEMStaff Inc.