A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Quartz Etching
Quartz Etching
2007-05-17
Sreemanth M Uppuluri
2007-05-17
Gareth Jenkins
2007-05-17
Bill Moffat
2007-05-18
Andrea Mazzolari
2007-05-18
Kirt Williams
XeF2 Etching Silicon
2007-05-18
Bin Liu
2007-05-18
ChungHao Chen (Joseph)
2007-05-18
P.D. Floyd
2007-05-18
Kirt Williams
Fused Quartz Cleaning
2007-05-30
Sreemanth M Uppuluri
2007-05-30
Julie Houser
2007-05-31
shay kaplan
2007-05-21
Nodes Norbert
Quartz Etching
Nodes Norbert
2007-05-21
Hello Sreemanth.

It can happen that HF diffuses through the resist and etches the wafer
area underneath. Then the resist layer is removed as well.
If that is the case, thickness of resist layer should be increased. The
time for etching is limited.

Best Regards,

Norbert Nodes

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Sreemanth M Uppuluri
Sent: Donnerstag, 17. Mai 2007 22:38
To: [email protected]
Subject: [mems-talk] Quartz Etching

Hello All,

I am interested in etching quartz using photoresist as the mask. From a
reference I found that BHF etches quartz at high speed and does not
affect
Shipley series photoresist. But when I did perform the etch I found that
the
photoresist has all been removed by the BHF solution. Can you please let
me
know what is going wrong. I am presently not using PDMS adhesive layer
before coating photoresist on quartz. Could this be a reason?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
The Branford Group