MEMSnet Home: MEMS-Talk: silicon nitride etch by koh?!
Au-etchant attacking plated nickel
2007-05-21
Sven Holmström
2007-05-21
David Nemeth
silicon nitride etch by koh?!
2007-05-21
Andrea Mazzolari
2007-05-22
Jordi Teva
2007-05-22
Shay Kaplan
2007-05-22
IGOR KADIJA
2007-05-22
Kirt Williams
silicon nitride etch by koh?!
Andrea Mazzolari
2007-05-21
Hi all,
i deposited about 20nm of silicon nitride on a silicon wafer.
After patterning silicon nitride, i etched silicon in KOH (20%) at 100°C.
After about 2 hours etch, silicon nitride was completely removed!
I always knew silicon nitride perfecly mask against KOH etch!
What could be happened ?

Best regards,
Andrea
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Addison Engineering