A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Any pre-PECVD SiO2 clean procedure?
Any pre-PECVD SiO2 clean procedure?
2007-05-25
Steven Yang
Any pre-PECVD SiO2 clean procedure?
Steven Yang
2007-05-25
Hi All,
I am going to do PECVD SiO2 on some silicon samples for the future
hydrophobic surface modification with SAM (like OTS) materials. I am
looking for some pre-PECVD clean procedure for this process. Any
sugesstions? The silicon sample with native oxide layer, and I will
first Pirnha clean it. I am not sure whether the 5:1:1 H2O:H2O2:HCl
clean and the Buffered HF clean should be followed in this process.
Thanks.
Oh, BTW, does anyboday have any info about the effect of thickness of
PECVD SiO2 on finial hydrophobicity with SAM modification.

Thank you very much!

Regards,
Steven
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics