Drie support wafer
2007-06-14
ashwini jambhalikar
2007-06-14
[email protected]
2007-06-14
Jim Beall
2007-06-15
Xiaoguang Liu
2007-06-15
Jim Beall
2007-06-18
Xiaoguang Liu
2007-06-15
Xiaoguang Liu
(211) silicon wafers
2007-06-16
Andrea Mazzolari
Drie support wafer
[email protected]
2007-06-14
Ashwini:

We have used Fomblin synthetic oil in the past for these applications. Clean up
afterwards is as easy as using Simple Green detergent followed by rinse and dry.
Bob Henderson

-----Original Message-----
From: ashwini jambhalikar 
To: [email protected]
Sent: Wed, 13 Jun 2007 9:39 pm
Subject: [mems-talk] Drie support wafer

Dear Friends,

Can anybody suggest me a better option than cool grease, for through etching
in DRIE

The wafer to be through etched needs a support wafer, and I am always using
cool grease in between the support wafer and the actual wafer to be etched.

Cool grease removal is really a headache, it can break the delicateÂ
structures.

I have heard about something like conducting tapes, which can be usedÂ
instead of cool grease.

if anybody knows about it or any other better option, please let me know...
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
University Wafer
Addison Engineering