Au-Au bonding
Xiaoguang Liu
2007-06-18
Dear Heyshan

That sounds like a simple process. I wonder how much bonding area you had on
the sample. I guess the pressure is really important. Thanks

Best
Leo

On 6/17/07, Mendis, Heyshan  wrote:
> We bonded some samples around 250-300C on our flip chip machine with
> around 5-10N force for 2-5min. Make sure both surfaces are oxide free.
> You also could enhance the strength by heat threatment around 300C for
> 0.5-1hrs.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Addison Engineering
Nano-Master, Inc.