MEMSnet Home: MEMS-Talk: Isotropic silicon etch
Isotropic silicon etch
2007-06-27
Chilcott, Dan W
2007-06-27
Kirt Williams
2007-06-27
David Nemeth
2007-06-29
Chilcott, Dan W
Low temperture anodic bonding between glass and silicon
2007-06-27
Robert Lindegren
2007-06-27
[email protected]
2007-06-28
Shao Guocheng
Isotropic silicon etch
Chilcott, Dan W
2007-06-27
To All,

I am looking for a well controlled isotropic silicon etch for etching 2 um deep
features. I do not believe that a timed plasma etch would be controlled enough
for this application. I am looking for a control of better than 0.5 um from lot
to lot and across the wafer. Any ideas?

Thanks,
Dan Chilcott
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMS Technology Review