Dear all,

I am looking for helpful info regarding etching glass or quartz
substrate with higher etch rate and vertical sidewall. Traditional HF
etching gives isotropical etch and STS dry etch with F radical gives
slow etch rate, they are all not good for my case since I am etching
around 30-50um deep wells inside the substrate.

Anyone can share your experience? Or anyone can provide the information
of the vendor who can do this job.

Appreciate your help .

Michael

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics