2007-07-03
sokwon Paik
2007-07-03
Jesse D Fowler
2007-07-03
Jian Wang
2007-07-05
sokwon Paik
articles/case studies Sn Al Cu
2007-07-05
A.E.Reinhardt
2007-07-12
Morten Aarøe
2007-07-05
Michael D Martin
Platinum deposition problem
sokwon Paik
2007-07-03
I have hard time in depositing platinum.

  I tried three different size e-beam evaporator but all deposition result in my
PMMA resist damage.

  If resist continues damage, I should go with negative resist for EBL and need
to etch out the other area but I'm afraid whether I could get good resolution
(~10nm) with etching.

  How did you resolve the heat problem? I tried to reduce the evaporation rate
but it seems not very helpful.

  Thank you,

  Sokwon Paik
  Postdoctoral research associate
  Oak Ridge National Laboratory

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Harrick Plasma, Inc.
MEMS Technology Review