hi all

i am working on Si etching using TMAH.
I am using Si added TMAH (10wt%) with AP for Al protection. As desired, I
have found that protective layer is formed over AL pads.
I am facing the problem in removing this layer to get good electrical
contact.
Does any one have any clue for this situation.