A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: polymer fabrication
polymer fabrication
2007-07-06
hammouche khales
2007-07-06
emelianov
2007-07-09
Rashid, Mamun
anodic bonding and passivation layer thickness
2007-07-09
H.J. van der Linden
How to get a sheet of Cr film via E-beam evap.
2007-07-09
hung bost
2007-07-10
Shay Kaplan
2007-07-10
Anil Agiral
2007-07-10
Peter Svasek
redeposition of SiO2
2007-07-11
cal Bear
plasma etching of SiO2 and its selectivity over resists
2007-07-12
prabhu arumugam
plasma etching of SiO2 and its selectivity over resists
2007-07-12
Kirt Williams
Polystyrene bonding problem
2007-07-13
Rashid, Mamun
2007-07-13
Joseph Grogan
2007-07-13
Rashid, Mamun
polymer fabrication
emelianov
2007-07-06
Hello,
it's depend of the formula of your PDMS. A lot of no cured siloxanes are
highly fugitive and building films on all of the clean surfaces. This way
they are contaminating a clean room. But there are a few of PDMSs, witch are
special produced for a clean room production. Check you vendors (f. e. Dow
Corning, GE, Wacker Silicones and so one) to get specifications and product
data sheets.


With best regards,
Vitali Emelianov
-----------------------------

caesar research center
Group Microrobotics
Ludwig-Erhard-Allee 2
D-53175 Bonn, Germany

Tel. +49 (0) 228 9656 342
e-Mail: [email protected]
www.caesar.de/1677.0.html


-----Ursprüngliche Nachricht-----
Von: [email protected] [mailto:[email protected]] Im
Auftrag von hammouche khales
Gesendet: Freitag, 6. Juli 2007 03:59
An: [email protected]
Betreff: [mems-talk] polymer fabrication

Hellos all, I have some questions if there is one ho need to help me!
- i need to have some informations for polymer fabrciation (especially
using PDMS ),  and if there is contaminations problems with CMOS process?
- what the clean room class if we need to fabricate bio-chip (or
microfluidic devices)?
Thanks
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Nano-Master, Inc.
Harrick Plasma, Inc.