A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: anodic bonding and passivation layer thickness
polymer fabrication
2007-07-06
hammouche khales
2007-07-06
emelianov
2007-07-09
Rashid, Mamun
anodic bonding and passivation layer thickness
2007-07-09
H.J. van der Linden
How to get a sheet of Cr film via E-beam evap.
2007-07-09
hung bost
2007-07-10
Shay Kaplan
2007-07-10
Anil Agiral
2007-07-10
Peter Svasek
redeposition of SiO2
2007-07-11
cal Bear
plasma etching of SiO2 and its selectivity over resists
2007-07-12
prabhu arumugam
plasma etching of SiO2 and its selectivity over resists
2007-07-12
Kirt Williams
Polystyrene bonding problem
2007-07-13
Rashid, Mamun
2007-07-13
Joseph Grogan
2007-07-13
Rashid, Mamun
anodic bonding and passivation layer thickness
Anil Agiral
2007-07-10
Hi Heiko,

Did you try Spin on Glass :

http://ej.iop.org/links/rFX7FtpBR/7PdGtMMu3BGc8eyQav5vpA/jm7307.pdf

Anil Agiral
PhD student
MESA+ Institute for Nanotechnology,
University of Twente, The Netherlands


On 7/9/07, H.J. van der Linden  wrote:
>
> Hi All,
>
> I am making a microfluidic device for electrokinetic studies. The device
> will
> consist of a channel deep-etched into silicon and a top layer consisting
> of
> glass. I want to use anodic bonding to bond the device.
> Because I will use the device for electrokinetic studies I need to be able
> to
> apply high voltages over the liquid in the channel. A problem here is of
> course
> that the native oxide on the silicon wafer will breakdown causing a short
> circuit
> through the silicon wafer. Therefore I want to apply an insulation layer
> on
> the
> silicon before the bonding. This layer will most likely be an oxide.
> The insulating layer is likely to interfere with the anodic bonding
> process.
> Has anyone tried a similar process ? The parameters that I am most
> interested in
> are the thickness of the insulating layer and the voltage and temperature
> for
> the anodic bonding process.... Voltages that I expect to use are around 50
> -
> 250V.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
Nano-Master, Inc.
University Wafer