We've been evaporating 250nm thick layers of SiO2 (for antireflection
coatings) using an ebeam evaporator on GaN and on sapphire. The samples
appear fine when we unload them from the chamber but when we start
unmounting the GaN sample, cracking of the oxide occurs. The sapphire
sample remains fine. Any ideas? We tried a plasma ash before hand on
both samples but still saw the cracking and also made sure the samples
were in good contact (for thermal purposes) with the metal mount.
Thanks
--John, Boston University Photonics

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
Nano-Master, Inc.
The Branford Group