Mounting shadow masks
2007-07-10
Prasoon Joshi
2007-07-12
Kirt Williams
2007-07-13
shay kaplan
Mounting shadow masks
Kirt Williams
2007-07-12
I have used cyanoacrylate (super glue) to hold on shadow masks.
Apply a fraction of a drop with a toothpick so you don't get too much.

To remove, heat above about 300 C and it decomposes, leaving a dust. Just
wipe it off.
Acetone or MEK at room temperature might also work for removal.

    --Kirt Williams

----- Original Message -----
From: "Prasoon Joshi" 
To: 
Sent: Tuesday, July 10, 2007 1:13 PM
Subject: [mems-talk] Mounting shadow masks

> Hi,
>
> I have been using Transmission Electron Microscopy (TEM) Cu grids, as a
> shadow mask for e-beam evaporation. I use rubber cement to hold down the
> TEM grid. Can anybody suggest something other than rubber cement?
>
> I need something that is easy to put on and remove, since I need to
> position the TEM grid using micromanipulators.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
The Branford Group
Process Variations in Microsystems Manufacturing