Surface Charge problems in PMMA - Ebeam lithography !!
2007-07-14
madhav rao
2007-07-16
Indusekhar
Surface Charge problems in PMMA - Ebeam lithography !!
Indusekhar
2007-07-16
Hello Madhav
Please try to ground the substrate.This should discharge charge
accumulated in PMMA during E-beam writing.

Good luck.

Indusekhar