Hi all,

Aspect ratio might be achieved up to 1:20 using Bosch
process. But it seems that the aspect ratio achievable
decreases with height increases. Is there any
relationship between the aspect ratio and height in
theory or according to experience?

Thank you  in advance.

Best Regards,
Matthew King

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
MEMS Technology Review
Process Variations in Microsystems Manufacturing