Hello Everyone,
I have a superlattice structure with following layers in the order:

Au
Cr
PECVD oxide (135 nm)
Si/SiGe SL (0.5 um)
SiGe/SiGeC buffer (1 um)
Si wafer

I want to remove Au, Cr and PECVD oxide layers. I was wondering if anyone could
suggest me on what etchants to use so that they selectively remove Au, Cr and
PECVD oxide layers but not the other layers.
Thanks,

  Nitin Shukla
  PhD Candidate
  Nanoscale Energy Transport Laboratory
  Department of Mechanical Engineering
  Virginia Tech
  Blacksburg, VA 24061
  Tel No: 540-231-5579
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
The Branford Group
Process Variations in Microsystems Manufacturing