MEMSnet Home: MEMS-Talk: Re: Membrane deflection
Re: Membrane deflection
1998-08-02
Gokhan Percin
1998-08-02
[email protected]
1998-08-02
Jarlath McEntee
1998-08-03
Mattias Vangbo
1998-08-03
Eric Bonnotte
1998-08-03
Mark Sheplak
1998-08-03
Culver Jim X3146
1998-08-03
Robert Dean
1998-08-03
J. Jay McMahon
1998-08-03
Larry L. Howell
1998-08-03
Peter Will
1998-08-02
Gokhan Percin
1998-08-03
Mark Sheplak
1998-08-03
Peter Will
1998-10-05
Andrezej Prochaska
Re: Membrane deflection
[email protected]
1998-08-02
Check my doctoral thesis.  The solution is there.

Fariborz Maseeh-Tehrani
MIT
June 1990

Good luck.

Fariborz Maseeh
[email protected]
IntelliSense Corp
16 Upton Drive
Wilmington, MA 01887
www.intellis.com
978-988-8000
978-988-8001 fax


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing
MEMS Technology Review