MEMSnet Home: MEMS-Talk: Aluminum etchand request
Aluminum etchand request
2007-08-04
Mustafa Celik
2007-08-06
[email protected]
Aluminum etchand request
Mustafa Celik
2007-08-04
Hi all,

I am trying to pattern a thin film of Al which is
coated on top of Indium-Tin-Oxide(ITO)layer. However
widely used MF319 positive PR Developer demages the
ITO. I've also tried lift-off but the result was not
satisfactory. Could you suggest me an alternative Al
etchand which does not attact ITO ?

Thanks in advance...