MEMSnet Home: MEMS-Talk: Removing oxidised resist from gold surfaces
Removing oxidised resist from gold surfaces
2007-08-13
Yue Mun Pun, Jeffrey
2007-08-13
Michael D Martin
Removing oxidised resist from gold surfaces
Yue Mun Pun, Jeffrey
2007-08-13
Hi,
Due to the long time taken for Acetone at 70-80'C used to remove AZ9260 resist
via lift-off, I have attempted to use Piranha (H2SO4:H2O2 = 3:1) to remove some
small amounts of resist remaining on my wafer surface which has gold conductors
patterned on it.
However, after the Piranha treatment, I observed water-like droplets remaining
on the gold conductors, which I think are solubulized resist that have been
oxidized by the Piranha and stained on the gold surfaces.  The SiO2 surface
remains clean.
Can anyone tell me how I can remove these 'resist droplets', which have stained
on the gold condutors?

Mr. Jeffrey Mun Pun YUE
余文彬
Division of Bioengineering
E3A-07-02, Nanobioanalytics Lab
7 Engineering Drive 1
National University of Singapore
Singapore 117574
Tel: (65) 65166482, Fax: (65) 68723069
E-mail:  [email protected]
Website:  http://www.bioeng.nus.edu.sg/people/trau/Lab_index.htm
"The only thing necessary for evil to triumph is for good men to do nothing"
(Edmund Burke)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing