MEMSnet Home: MEMS-Talk: photoresist suggestion
SOI wafers
2007-08-14
[email protected]
photoresist suggestion
2007-08-15
Andrea Mazzolari
2007-08-16
Bill Moffat
2007-08-17
Isaac Chan
2007-08-18
Hongzhi CHEN
photoresist suggestion
Bill Moffat
2007-08-16
Do not spin the primer.  Use a vacuum vapor primer for total resist adhesion.
If you can not locate one contact me for a free test.

Bill Moffat, CEO
Yield Engineering Systems, Inc.
203-A Lawrence Drive, Livermore, CA  94551-5152
(925) 373-8353

[email protected]

-----Original Message-----
From: [email protected] [mailto:[email protected]] On
Behalf Of Andrea Mazzolari
Sent: Wednesday, August 15, 2007 3:19 PM
To: [email protected]; General MEMS discussion
Subject: [mems-talk] photoresist suggestion

Hi all, i need to pattern a 400um thick silicon nitride film.
I'm planning to use BHF (1:7) to remove silicon nitride from unwanted areas.
Etch rate of silicon nitride is about 1nm/min, so the etch time will be about
400 min.
About photoresist: i've tried to use s1813, but it peel off after about 5 hours
etch.

Here is the procedure i've followed:
spinning of primer
spinning of s1813
soft bake (2 min at 120 °C)
photolitography
hard bake (2 min at 120 °C)

How can i improve s1813 resistance to BHF? May a thicker s1813 layer help ? Or a
longer hard bake time ?
Any idea about an alternative photoresist ?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
Mentor Graphics Corporation
Addison Engineering