robust
lines SU-8 sidewall
robust
2007-08-17
I experienced that as I develop holes array and it may be caused by over
exposure or too long time PEB. developing with strong Agitation, such as
ultrusonic or megasonic might help if you do not like adjust your other
processes.

Regards!

Xiao Qiang

  _____

From: [email protected] on behalf of Chen Han Lee
Sent: Fri 8/17/2007 7:11 AM
To: [email protected]
Subject: [mems-talk] lines SU-8 sidewall

Hi Colleagues,

I am using su-8 to build thick structures,
have anyone experience vertical lines on the walls of the su-8 structures?
what are they called and what caused them?

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
University Wafer
Nano-Master, Inc.