Ag deposition on Si
2007-08-20
Vikrant A. Chaudhari :)
2007-08-21
Jesse D Fowler
2007-08-27
Kirt Williams
Ag deposition on Si
Jesse D Fowler
2007-08-21
I've evaporated it, using a Cr adhesion layer. What do you want to know?

Jesse Fowler


"Vikrant A. Chaudhari writes:

> hello friends,
>
> has any one tried Ag deposition on Si
>
> vikrant