MEMSnet Home: MEMS-Talk: Lift-off Process for High Density Metal Electrodes (5-10 microns separation)
Lift-off Process for High Density Metal Electrodes (5-10 microns separation)
2007-08-22
AKM Newaz
Lift-off Process for High Density Metal Electrodes(5-10 microns separation)
2007-08-22
Bill Moffat
III-V semiconductor wet etch
2007-08-22
Andrea Mazzolari
Lift-off Process for High Density Metal Electrodes(5-10 microns separation)
2007-08-22
Roger Shile
Lift-off Process for High Density Metal Electrodes (5-10 microns separation)
AKM Newaz
2007-08-22
Dear All,

           I am designing a photomask for a high density metal electrodes.
They electrodes are 2 microns of width, 5 mm long  and separated by 5~10
microns. I am planning for 200 nm of Ti/Au metal. The first question will be
should I use image reversal (AZ5214 using bright field mask) or bi-layer
photoresis (LOR+S1813 using dark field mask)? OR should I use completely
different photoresist? I found in the mems-talk archive that bi-layer
photoresist has some problem for high density electrodes. Any suggestion
will be highly appreciated. Thanks in advance.

Newaz
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering