MEMSnet Home: MEMS-Talk: Degradation of PECVD Si3N4 film after SU-8 wafer level adhesive bonding
Degradation of PECVD Si3N4 film after SU-8 wafer level adhesive bonding
2007-08-27
Chih-Chieh Cheng
Degradation of PECVD Si3N4 film after SU-8 wafer level adhesive bonding
Chih-Chieh Cheng
2007-08-27
Hi

We have fabricated MIM structures (Au-PECVD Si3N4-SiCr) and found that the
leakage current of Si3N4 was incrediblely increased after SU-8 adhesive
bonding. We used semi-crossed linked SU-8 as the adhesive layer so that we
can create cavities on the bottom wafer and bond to MIM structure on
the bottom wafer. The SU-8 layer was right on the top of the Au layer after
bonding. The bonding temp was ramped up to 150 degree C with the applied
force 2000 NT over the 4" fused quartz wafer for 1hr. Could anyone share
with your insightful comments on the degradation of Si3N4 layer?

Thanks

Chih-Chieh
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Addison Engineering
Mentor Graphics Corporation
Nano-Master, Inc.