Hi,
I am trying to coat AZ9260 on polymerised SU-8 2005 in order to pattern gold
conductors on the SU-8.  Has anyone had any experience on this before?  It seems
that the AZ9260 keeps spinning off the SU-8 when I use 2100rpm for 60s.

Jeffrey