A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: RIE Question
Probe Arms with Kinematic bearings? Where to buy it?
2007-08-30
Guangchi Archie Xuan
RIE Question
2007-08-30
Joseph Grogan
2007-08-30
Michael D Martin
2007-08-31
PRAMOD GUPTA
2007-09-04
Bill Moffat
2007-08-30
[email protected]
2007-09-02
Nicolas Duarte
RIE Question
Joseph Grogan
2007-08-30
Hi All,

We have a very old Plasmalab RIE in our facility that I tried using to
etch a Si wafer patterned with 1813 resist. I used the following parameters:

02 flow rate: 5 sccm
SF6 flow rate: 20 sccm
pressure: 20 mT
power: 150 W
time: 1 hr

I had hoped to get a depth in the neighborhood of 60um or more with
these settings (based on literature such as Williams' etch rates paper).
Unfortunately, I only got around 4.5 um deep, and that was only in the
center 2" of my 4" wafer. The outer 2" of my wafer was coated in an odd
white chalky film that smudged off a little if I wiped it.

Does anyone have a guess as to what my problem is?

thanks,
Joe Grogan
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
MEMStaff Inc.
University Wafer